The beginning of the process is characterized by smooth (adjustable) increase the wire feed speed (Fdc) before touching the wire welding products. High short-circuit current, attributable to too small area of the cross section of cold welding wire leads welding transformer power supplies to chaotic,uncontrolled excitation of the arc, which is the main reason of defects in the beginning of the weld and in the places where they overlap. The inverter devices DSP processor delay time finding a power source in short circuit mode, thus giving the wire to heat up, and then gradually decreases in current to welding, providing a «soft start» and defects in the beginning of the joint.